Gilsonite Metal Content and Trace Element Analysis
Gilsonite metal content is low for a reason: gilsonite is a solid hydrocarbon resin, not a mined ore, and its trace metal profile reflects that. The analysis reports mercury at 0.004 ppm, lead at 0.8 ppm and cadmium below 0.4 ppm. In short, this page gives the full elemental analysis in both percent and ppm, then reads those figures against the limits that actually get applied in purchasing — US offshore discharge rules, RoHS and the EU toy safety limits — including the two elements where this analysis does not settle the question on its own.
Figures as reported on the elemental analysis for RAHA Gilsonite. Trace metal content is a property of the deposit and the batch, so a batch certificate should always accompany a shipment where compliance is being claimed.

Gilsonite metal content: the full analysis
The table below gives every element on the analysis. The first column reproduces each figure exactly as the laboratory issued it. The second converts that figure to parts per million, because purchasing specifications and regulatory limits use ppm rather than percent. Since one percent equals 10,000 ppm, the conversion stays arithmetic and reversible — nothing here has been rounded or adjusted.
| Element | As reported | Equivalent (ppm) | Notes |
|---|---|---|---|
| Manganese (Mn) | <0.0008% | <8 | Below detection |
| Copper (Cu) | <0.0008% | <8 | Below detection |
| Zinc (Zn) | <0.0004% | <4 | Below detection |
| Cobalt (Co) | 0.004% | 40 | Measured value |
| Nickel (Ni) | 0.004% | 40 | Measured value |
| Chromium (Cr) | <0.0008% | <8 | Total chromium |
| Thallium (Tl) | <0.001% | <10 | Below detection |
| Barium (Ba) | <0.002 | <20 † | Unit not stated — see note |
| Selenium (Se) | <0.04% | <400 ‡ | High detection limit |
| Bismuth (Bi) | <0.008% | <80 | Below detection |
| Antimony (Sb) | <0.008% | <80 | Below detection |
| Beryllium (Be) | <0.0008% | <8 | Below detection |
| Mercury (Hg) | 0.004 ppm | 0.004 | Measured value |
| Lead (Pb) | 0.8 ppm | 0.8 | Measured value |
| Cadmium (Cd) | <0.4 ppm | <0.4 | Below detection |
| Arsenic (As) | <4.0 ppm | <4.0 | Below detection |
† Barium is reported on the source analysis without a unit. It is shown here as a percentage in line with the adjacent rows; confirm it against the batch certificate before using it in a specification.
‡ The selenium detection limit sits an order of magnitude above the others in the table. Treat it as a reporting limit for that method rather than as an indication of selenium content, and request a lower-limit determination if selenium is critical to your application.
How to read these figures
Three things about this table change how you should use it, and readers routinely misread all three.
“Less than” means not detected, not zero
Eleven of the sixteen rows carry a less-than sign. There, the laboratory is stating that it did not find the element above the limit its method could resolve. That does not mean the element is absent. Nor does it mean the true value sits near the limit — in fact the actual content may be far lower. For a compliance file, therefore, quote the detection limit itself, because that is the strongest statement the analysis supports.
Percent and ppm are the same information
Most rows carry a percentage and four carry ppm directly. Laboratory reports mix the two units routinely, and that mixture causes most specification errors: 0.004% means 40 ppm, while 0.004 ppm is ten thousand times smaller. For example, cobalt and nickel at 0.004% sit four orders of magnitude above mercury at 0.004 ppm, although at a glance the two figures look identical. So always carry the unit through.
Total content is not migration or leachate
Every figure here gives total content in the solid resin, measured after digestion. However, several of the limits buyers work to — toy safety, food contact, soil leaching — are migration or leachate limits, which measure what comes out of the material under a defined extraction. Total content below a migration limit settles the question, because nothing can migrate that is not there. By contrast, total content above a migration limit proves nothing either way and needs the extraction test run.
Why trace metals in gilsonite matter
Gilsonite goes into drilling fluids, printing inks, paints, asphalt and foundry sand binders. In three of those five, somebody downstream is running a heavy metals test, and the question reaching the supplier is always the same: will this additive put my finished product over a limit?
Drilling fluids and offshore discharge
Regulators control water-based muds discharged offshore on the metal content of their components, and barite normally decides the outcome — a mined sulfate ore that can carry mercury and cadmium straight from the deposit. Mud systems, meanwhile, take gilsonite at only a few pounds per barrel as a shale stabiliser and fluid loss control agent, so its contribution to the total metal load in the mud is small to begin with. The figures above show why it stays small. See the comparison in the next section.
Printing inks and packaging
Printing ink uses gilsonite as a hydrocarbon resin and black pigment extender. Because inks printed on food packaging must meet migration limits on heavy metals, ink makers hold a declaration for every raw material in the formulation. Lead at 0.8 ppm and cadmium below 0.4 ppm are the two figures they request most often for that file.
Paints, coatings and consumer products
In paints and stains, RoHS drives anything going into electrical equipment, while the toy safety limits drive anything that may reach children. Both sections follow below. Of the two, only the toy safety case needs this analysis supplemented.
Foundry and asphalt
In foundry sand the concern turns on emissions during pouring rather than on the metal content of the binder. Similarly, asphalt modification uses low dosage in a bound matrix. Neither application normally triggers a heavy metals specification, although buyers still request the data as part of a general supplier qualification.
Gilsonite against the US offshore discharge limits
The clearest external benchmark for a drilling fluid additive is the US effluent guideline for offshore oil and gas extraction. It sets maximum metal content for stock barite used in discharged muds: mercury at 1 mg/kg dry weight and cadmium at 3 mg/kg dry weight.
The regulation writes those limits for barite rather than for gilsonite, so treat the comparison as a reference point and not as a compliance test. Even so, mud engineers use exactly this reference point, because the permit carries that number.
| Element | Gilsonite, reported | Stock barite limit | Margin |
|---|---|---|---|
| Mercury | 0.004 mg/kg | 1 mg/kg | 250× below |
| Cadmium | <0.4 mg/kg | 3 mg/kg | at least 7.5× below |
Mercury makes the more striking case of the two. At 0.004 mg/kg, gilsonite sits two and a half orders of magnitude under a limit that barite suppliers must actively manage by selecting deposits. The cadmium margin, on the other hand, states a floor rather than a figure: the true content falls somewhere below 0.4 mg/kg, so 7.5× is simply the smallest margin the analysis can support.
For a mud formulator, therefore, adding gilsonite to a water-based system does not move the mud’s metal loading in any direction that matters. The decision stays with the barite.
Gilsonite against RoHS
RoHS restricts four metals in materials that go into electrical and electronic equipment, setting maximum concentration values by weight in homogeneous material: lead 0.1%, mercury 0.1%, cadmium 0.01% and hexavalent chromium 0.1%. In ppm terms those limits are generous, since 0.1% means 1,000 ppm.
| Element | Gilsonite, reported | RoHS limit | Margin |
|---|---|---|---|
| Lead | 0.8 ppm (0.00008%) | 1,000 ppm (0.1%) | 1,250× below |
| Mercury | 0.004 ppm | 1,000 ppm (0.1%) | 250,000× below |
| Cadmium | <0.4 ppm | 100 ppm (0.01%) | at least 250× below |
| Chromium VI | not speciated; total Cr <8 ppm | 1,000 ppm (0.1%) | bounded at 125× below |
The chromium row deserves a word, because buyers question it most often. The analysis reports total chromium rather than the hexavalent fraction that RoHS restricts. That still settles the matter here: hexavalent chromium forms part of total chromium, so it cannot exceed total chromium. With total chromium below 8 ppm against a limit of 1,000 ppm, the material clears the restriction whatever the speciation turns out to be. However, the same logic fails where the limit sits tighter than the total — which is exactly the situation in the next section.
Gilsonite and the EU toy safety limits: where it clears and where it does not
The EU Toy Safety Directive sets migration limits for a long list of elements. For dry, brittle, powder-like or pliable material — the category a resin powder would fall into — the relevant values are lead 2.0 mg/kg, cadmium 1.3 mg/kg, arsenic 3.8 mg/kg, mercury 7.5 mg/kg, chromium III 37.5 mg/kg and chromium VI 0.02 mg/kg.
These are migration limits, which measure what leaches out under a defined extraction, so the reasoning from the previous section applies: where total content already sits below the migration limit, the material cannot fail. Otherwise the extraction test has to settle it.
| Element | Gilsonite, total | Migration limit | Outcome |
|---|---|---|---|
| Lead | 0.8 mg/kg | 2.0 mg/kg | Clears on total content |
| Cadmium | <0.4 mg/kg | 1.3 mg/kg | Clears on total content |
| Mercury | 0.004 mg/kg | 7.5 mg/kg | Clears on total content |
| Chromium III | <8 mg/kg total Cr | 37.5 mg/kg | Clears on total content |
| Arsenic | <4.0 mg/kg | 3.8 mg/kg | Not resolved — migration test required |
| Chromium VI | <8 mg/kg total Cr | 0.02 mg/kg | Not resolved — speciation required |
This analysis settles four of the six on its own. Two it does not, and the reason in each case is worth stating exactly.
Arsenic
The reported arsenic detection limit falls below 4.0 mg/kg, while the migration limit stands at 3.8 mg/kg. Because the detection limit sits just above the regulatory limit, the analysis cannot demonstrate compliance — even though the true arsenic content very likely falls well under it. In other words, the reporting limit creates this gap, not the material. Either a determination with a lower detection limit or an actual migration test to the toy safety method resolves it.
Hexavalent chromium
The chromium VI migration limit of 0.02 mg/kg falls far below the total chromium detection limit of 8 mg/kg, so the bounding argument that worked for RoHS fails here. A reduced organic matrix such as an asphaltite resin rarely holds hexavalent chromium, but rarely is not a test result. If the application is a children’s product, therefore, run a speciated analysis.
For every other use of gilsonite — drilling, asphalt, ink, paint, foundry — neither of these two points arises, because the toy safety limits do not apply.
What this analysis does not cover
A metal content sheet answers one narrow question. Yet buyers regularly assume it covers four further things, and it covers none of them.
Polycyclic aromatic hydrocarbons
PAH content is not a metal determination, so this analysis does not carry it. It takes a separate test on a separate method. Where a regulation restricts PAH in your application, therefore, request that determination specifically, and never read a clean metals sheet as a statement about PAH.
Vanadium and iron
Neither element appears on this analysis, although buyers ask about both routinely — vanadium because it is the characteristic metal of petroleum-derived residues and the first thing a refinery buyer checks, iron because it shifts colour in ink and paint applications. If either matters to your specification, request them as an addition rather than inferring anything from their absence here.
Sulfur
Gilsonite carries sulfur at percentage level rather than trace level, so it belongs on the main specification rather than on a trace metals sheet. See the chemical characterisation page for the elemental composition of the resin itself.
The analytical method
The figures as issued name neither the method nor the digestion. For a compliance file the method matters as much as the result, so ask for a batch certificate that names the method, the digestion and the detection limits.
Why gilsonite is low in trace metals
The figures above reflect what the material is rather than any quality achievement — and that distinction explains why the numbers stay stable from batch to batch.
Gilsonite is a solid hydrocarbon — an asphaltite that filled near-vertical fractures in the host rock as a migrating fluid, then hardened in place. Metals enter a mineral deposit by three routes: sulfide mineralisation, substitution in a crystal lattice, or adsorption onto clay. However, a fracture-fill hydrocarbon resin offers none of them. It holds no sulfide phase for mercury and cadmium to sit in, no sulfate lattice of the kind barite has, and no clay fraction at all.
Two elements do show a measured value rather than a detection limit — nickel and cobalt, both at 40 ppm — and they behave that way for a reason. Nickel and cobalt coordinate into porphyrin structures in organic matter, the one mechanism by which a hydrocarbon genuinely does concentrate a metal. So finding them at tens of ppm while the sulfide-associated metals stay below detection is the signature of an organic deposit rather than a mineral one.
For the same reason, the comparison with barite earlier is chemistry rather than marketing. Barite is a mined sulfate ore and carries whatever its deposit carried, while gilsonite is a hydrocarbon and simply lacks the chemistry to hold those metals. The molecular structure page covers the resin chemistry in more detail.
Getting a batch-specific certificate
Gilsonite metal content varies with the deposit and the working face, so a figure on a website is a typical value and not a guarantee for the container you are buying. Where metal content is written into a purchase specification, three things are worth insisting on.
First, ask for a certificate against the shipment rather than a generic sheet, with the batch or lot identified on it. Second, ask for the detection limits alongside the results, because a result of “not detected” is only as strong as the limit behind it. Finally, where the figure is contractual, let the inspection company run the determination instead of the supplier’s own laboratory.
Independent inspection at loading can be arranged on request — SGS, Bureau Veritas, Intertek or the surveyor named in your contract.
Supply and commercial terms
RAHA Gilsonite supplies gilsonite in lump, powder and micronized grades, with the grade selected on ash, softening point and mesh rather than on metal content, which does not vary meaningfully between them.
| Payment | 50% TT in advance, balance agreed with the order |
|---|---|
| Incoterms | FOB, CFR or CIF |
| Loading ports | Jebel Ali or Mersin |
| Minimum order | One full 20′ container |
| Lead time | Quoted per destination |
| Documentation | Specification sheet, SDS and batch certificate |
Send the elements and the limits you are working to, with the standard they come from, and the available determination can be checked against them before any order is placed.
Regulatory limits quoted on this page
Every limit used for comparison above comes from a published source rather than from an interpretation. They appear here so that you can check the arithmetic yourself.
- Stock barite, mercury 1 mg/kg and cadmium 3 mg/kg dry weight — US effluent limitations for the offshore subcategory of oil and gas extraction, 40 CFR § 435.13
- RoHS maximum concentration values — lead 0.1%, mercury 0.1%, cadmium 0.01%, hexavalent chromium 0.1% by weight in homogeneous material, Directive 2011/65/EU
- Toy safety migration limits, dry and powder-like material — lead 2.0, cadmium 1.3, arsenic 3.8, mercury 7.5, chromium III 37.5 and chromium VI 0.02 mg/kg, Annex II of Directive 2009/48/EC as implemented by EN 71-3
Regulations are amended. Verify the current text against the official source before relying on any limit for a compliance decision, and note that the barite limits are written for barite rather than for gilsonite and are used here only as a reference point.
Frequently asked questions
Reading the analysis
What is the metal content of gilsonite?
On the elemental analysis for RAHA Gilsonite, mercury is 0.004 ppm, lead is 0.8 ppm, cadmium is below 0.4 ppm and arsenic is below 4.0 ppm. Nickel and cobalt are the highest reported at 40 ppm each. Eleven of the sixteen elements on the analysis are below the detection limit of the method.
Does gilsonite contain heavy metals?
Only at trace level. The metals that are actually measured rather than reported below detection are nickel and cobalt, at 40 ppm each, which enter organic matter through porphyrin coordination. The metals that cause regulatory problems in mined minerals — mercury, cadmium, lead — are present at parts per billion to sub-ppm level, because a hydrocarbon resin has no sulfide or lattice chemistry to hold them.
What does “less than 0.0008%” mean on the analysis?
It means the element was not detected above 8 ppm, which is the lowest concentration that method could resolve. It is not a measurement of 8 ppm and it is not a statement that the element is absent. For a specification, the detection limit is the reportable figure because it is the strongest claim the analysis supports.
Why is the selenium figure so much higher than the others?
The selenium detection limit of 0.04% is roughly ten to a hundred times higher than the limits for the surrounding elements. That reflects the sensitivity of the method for selenium rather than the selenium content of the material. If selenium is critical to your specification, request a determination with a lower reporting limit.
Compliance and regulatory limits
Is gilsonite RoHS compliant?
The reported figures sit far below all four RoHS maximum concentration values: lead 1,250 times below, mercury 250,000 times below, cadmium at least 250 times below. The analysis does not speciate hexavalent chromium, but total chromium below 8 ppm against a limit of 1,000 ppm bounds it conclusively. Still issue the RoHS declaration against the batch rather than against a published figure.
Can gilsonite be used in a children’s product or toy?
Total content alone clears four of the six relevant toy safety elements. Two are not. The arsenic detection limit of 4.0 mg/kg sits just above the 3.8 mg/kg migration limit, and the hexavalent chromium migration limit of 0.02 mg/kg is well below the total chromium detection limit of 8 mg/kg. Both need a determination with lower limits, or an actual migration test, before anyone can claim compliance.
Is total content the same as leachable or migratable content?
No. Every figure here is total content in the solid resin after digestion. Toy safety, food contact and soil leaching limits are extraction-based. Total content below an extraction limit is conclusive, because nothing can leach that is not present. Total content above it proves nothing and requires the extraction test.
Drilling fluids and the comparison with barite
How does gilsonite compare with barite on mercury and cadmium?
The US offshore effluent guideline caps stock barite at 1 mg/kg mercury and 3 mg/kg cadmium. Gilsonite comes in at 0.004 mg/kg mercury, 250 times under that cap, and below 0.4 mg/kg cadmium, at least 7.5 times under. Barite is a mined sulfate ore and carries deposit metals; gilsonite is a hydrocarbon resin and does not.
Does adding gilsonite to a water-based mud affect its metal loading?
Not materially. Mud engineers dose gilsonite at a few pounds per barrel, and its metal content sits orders of magnitude below the limits that apply to mud components. The barite decides the metal loading of a water-based mud, because it goes in at far higher concentration and carries far higher metal content.
What the determination does not cover
Does this analysis cover PAH content?
No. Polycyclic aromatic hydrocarbons are not metals, and a separate method determines them. So a clean trace metal analysis says nothing about PAH content. Where a regulation restricts PAH in your application, request that determination specifically.
Why are vanadium and iron not on the analysis?
They were not included in the determination. Vanadium is the characteristic metal of petroleum-derived residues and iron affects colour in ink and paint, so both are commonly requested. Their absence from this sheet is not a result, and a batch determination can include either one on request.
Grades, batches and documentation
Does metal content vary between lump, powder and micronized grades?
Not meaningfully. Grading is a size reduction of the same resin, so the trace metal profile carries through. Ash content, softening point and mesh drive grade selection, not metal content.
Does metal content vary between batches?
Trace metal content follows the deposit and the working face, so figures move within a narrow band rather than staying fixed. The elements that sit below detection stay below detection; nickel and cobalt are the two that shift. Where the figure is contractual, work from a batch certificate rather than a published typical value.
Can the determination be done by an independent laboratory?
Yes. Independent inspection at loading can be arranged on request — SGS, Bureau Veritas, Intertek or the surveyor named in the contract. Where a metal limit is written into a purchase specification, an independent determination is the sensible route.
What documentation comes with a shipment?
Specification sheet, safety data sheet and batch certificate. Where a metal content declaration is needed for a regulatory file, say which standard and which elements when ordering so the right determination is run on the batch.
Related technical pages
- Gilsonite specification — ash, softening point, moisture, volatile matter and mesh
- Chemical characterisation — carbon, hydrogen, nitrogen, sulfur and oxygen content
- Molecular structure — the resin chemistry behind the metal profile
- Safety data sheet — handling, exposure and transport classification
- Drilling fluid additives — the full range for mud systems